IDENTIFICATION
Gemet 817, ENiCrCoMo-1
CLASSIFICATION
AWS/SFA 5.11: ENiCrCoMo-1, EN/ISO 14172: ENi6617
NiCr22Co12Mo, DIN: 1736 ENiCr21 Co12Mo, UNS: W86117
DESCRIPTION
Nickel base basic coated electrode, with an alloyed core wire depositing weld metal having about 22 Cr-10 Co-9 Mo-55 Ni. The weld metal has excellent resistance to corrosion and high temp oxidation in the range 800° C to 1150° C. The electrode can be used in positional welding and meets radiographic quality requirements.
WELD METAL ANALYSIS (RANGE) %
C | Mn | P | S | Si | Cu | Fe | Ni | Cr | Co | Mo | Nb + Ta |
0.05 - 0.15 | 0.5 - 2.5 | 0.03 | 0.015 | 1 | 0.5 | 5 | Remainder | 21.0 - 26.0 | 9.0 - 15.0 | 8.0 - 10.0 | 1 |
max | max | max | max | max | max |
MECHANICAL PROPERTIES (RANGE)
UTS (MPa) | EL (%) (L=4D) | CVN Impact Value | |
620 min | 25 min | Temp | Joules |
+ 20°C | 90 min |
TYPICAL APPLICATIONS
BASE MATERIALS
UNS | Alloy | DIN | Material N° |
N08810 | 800H | X5NiCrAlTi3120 | 1.4958 |
DS | X8NiCrSi3818 | 1.4862 | |
N06601 | 601 | NiCr23Fe | 2.4851 |
N06617 | 617 | NiCr23Co12Mo | 2.4663 |
SPECIAL INSTRUCTIONS
• Rebaking: 1 hour at 250° - 300°C.
• Joints to weld must be clean, exempt from grease, cracks.
• Guide electrodes with a slight declination, weld with a short arc and prevent a high heat input by applying the stringer bead technique (weaving max. 2 times core wire diameter)
• Nickel base alloys are welded without preheating and a interpass temperature <150°C. For repair welding of steels with high carbon content a preheating between 200 - 500°C has to be applied. A post weld heat treatment can be performed without influence on the weld deposit
PACKING PARAMETERS
Size (mm) | Length (mm) | Current Condition Amps DC (+) | Packing / Packet (Kg) | Packing / Box (kg) |
2.5 | 300 | 50 - 70 | 2 | 2 x 5 = 10 |
3.15 / 3.20 | 350 | 70 - 100 | 2 | 2 x 5 = 10 |
4 | 350 | 90 - 130 | 2 | 2 x 5 = 10 |