IDENTIFICATION
Gemet 825N, ENiCrMo-3
CLASSIFICATION
AWS SFA 5.11 ENiCrMo3
DIN 1736 EL-NiCr20Mo9Nb (2.4621)
DESCRIPTION
Medium heavy coated, basic type, nickel base electrode intended for welding Inconel 625 and similar composition alloys which are primarily used for their excellent corrosion and oxidation resistance.
They exhibit an exceptionally high resistance to pitting corrosion and chloride induced stress corrosion cracking. The electrode is manufactured using nickel-alloyed core wire and hence it is non-synthetic The deposited welds are of x-ray quality.
WELD METAL ANALYSIS (RANGE) %
C | Mn | Si | S | P | Cb + Ta | Cu | Cr | Ni | Mo | Fe |
0.09 | 1 | 0.20 - 0.75 | 0.015 | 0.02 | 3.15 - 4.15 | 0.5 | 20.0 - 23.0 | 55 | 8.0 - 10.0 | 1.5 |
Max | max | max | max | max | min | max |
MECHANICAL PROPERTIES (RANGE)
UTS (N/mm2 ) | EL (%) (L=4D) | Bend Test Results | CVN Impact Value | |
Temp | Joules | |||
770 - 890 | 30 – 50 | Satisfactory | -196°C | 40 - 100 |
TYPICAL APPLICATIONS
FERRITE CONTENT : FN-O (WRC-92)
INTERPASS TEMPERATURE : 100°C max.
HEAT IN-PUT : 1.5 kJ/mm max.
SCALING TEMPERATURE : 1100°C (air)
CORROSION RESISTANCE
Very good resistance to general and inter-granular corrosion. Maximum resistance (practically immune) to pitting corrosion, crevice corrosion and stress corrosion cracking in chloride bearing environments.
PACKING PARAMETERS
Size (mm) | Length (mm) | Current Condition DC (+) Amps | Packing / Packet (kg) | Packing / Box (kg) |
2.5 | 350 | 60 - 80 | 2 | 2 x 5 = 10 |
3.15 / 3.20 | 350 | 70 - 120 | 2 | 2 x 5 = 10 |
4 | 350 | 100 - 155 | 2 | 2 x 5 = 10 |
5 | 350 | 130 - 250 | 2 | 2 x 5 = 10 |