Getig 904L, ER 385

CLASSIFICATION
AWS/SFA-5.9 ER 385 BS 2901-90 904S92
DIN 8556 WSGX2CrNiMoCuN 20.25

DESCRIPTION

Solid wire which gives a “904L” type fully austenitic deposit. The wire gives a low carbon nil ferrite “super- austenitic” weld metal with good resistance to attack by a range of organic and inorganic acids, and better resistance to pitting attack than 317L type.

CHEMICAL ANALYSIS (RANGE) %

C Mn Si S P Cr Ni Mo Cu
0.025 max 1.0 - 2.50 0.25 - 0.65 0.015 0.015 19.5 - 21.5 24 - 26 4.20 - 5.20 1.2 - 2.0
max max

MECHANICAL PROPERTIES (RANGE)

TS (N/mm²) EL (%) (L=4D) CVN Impact Value
    Temp Joules
660 min 40 min -196°C 50

TYPICAL APPLICATIONS

  • Corrosion resistance steels of the “904L” type ASTM UNS N08094 DIN 1.4500 (Cast), 1.4539.
  • Widely used in chemical process plant, particularly in phosphoric and Sulphuric acid, fertilizer and acetic acid production.

CORROSION RESISTANCE

Very good resistance to general and intergranular corrosion in non-oxidating acid environments e.g. Sulphuric upto 90%, phosphoric and organic acids. Good resistance to stress corrosion cracking and pitting corrosion in chloride bearing environments.

SHIELDING GAS : Pure Argon 99.9% 6-12 l/mn.

WELDING CURRENT : DC ( - )

SCALING TEMPERATURE : Approximately 1000°C in air

PACKING PARAMETERS

Size (mm) Length (mm) Packing / Packet (kg) Packing / Box (kg)
1.6 1000 5 5 x 4 = 20
2 1000 5 5 x 4 = 20
2.40 / 2.50 1000 5 5 x 4 = 20
3.15 / 3.20 1000 5 5 x 4 = 20