IDENTIFICATION
GM 307Si
CLASSIFICATION
EN 14343 (EN 12072, G 18 8 Mn)
DESCRIPTION
The wire gives a strong, ductile and tough austenitic deposit, which works-hardens from about 200HV to 450HV. Also compatible with cast iron in some applications. The addition of about 6% Mn gives good crack resistance in difficult highly restrained joints.
CHEMICAL ANALYSIS (RANGE) %
C | Mn | Si | Cr | Ni | Cu | Mo | S | P |
0.2 max | 05-Aug | 0.60 - 1.20 | 17 - 20 | 07-Oct | 0.3 max | 0.3 max | 0.03 max | 0.03 max |
MECHANICAL PROPERTIES (RANGE)
UTS (MPa) | EL (%) | CVN Impact Value | |
Temp | Joules | ||
590 min | 30 min | -50°C | 95 |
TYPICAL APPLICATIONS
SHIELDING GAS : Ar + 2 % O2 , Ar + 5 - 20 % CO2
WELDING MODE : (=+)
PACKING PARAMETERS
Welding Parameters | |||
Size (mm) | Pulsed arc (A) | (V) | Weight / Spool (kg) |
0.8 | 100 - 150 | 22 - 27 | 12.5 / 15.0 |
1 | 120 - 200 | 24 - 28 | 12.5 / 15.0 |
1.2 | 140 - 220 | 24 - 28 | 12.5 / 15.0 |
1.6 | 180 - 260 | 24 - 30 | 12.5 / 15.0 |