IDENTIFICATION
GM 821, ERNiCr3
CLASSIFICATION
AWS/SFA 5.14: ERNiCr3, BS 2901-90 NA 35,
DIN 1736- 85WSGNiCr2ONb Worst-off no 2.4806
DESCRIPTION
GM 821 is intended for welding Inconel 600 and similar composition alloys. The deposit tolerates high dilution levels and is very resistant to hot cracking. It is not susceptible to sigma phase embitterment or carbon migration and is therefore ideal for service at elevated temperatures. The weld metal passes X-ray quality.
CHEMICAL ANALYSIS (RANGE) %
C | Cr | Mn | Si | S | P | Ti | Cu | Fe | Nb + Ta | Ni |
0.1 | 18.0 - 22.0 | 2.5 - 3.5 | 0.5 | 0.015 | 0.03 | 0.75 | 0.5 | 3 | 2.0 - 3.0 | 67 |
max | max | max | max | max | max | max | min |
MECHANICAL PROPERTIES (RANGE)
TS (N/mm²) | YS (N/mm²) | EL (%) (L=4D) | CVN Impact Value | |
Temp | Joules | |||
550 - 690 | 360 - 510 | 30 - 45 | -196°C | 60 - 120 |
TYPICAL APPLICATIONS
FERRITE CONTENT : FN 0
CORROSION RESISTANCE : Extremely good resistance to general and intergranular corrosion and very good resistance to stress corrosion cracking.
HIGH TEMPERATURE PROPERTIES : Resistance to oxidation in air upto 1150ºC, in sulphur dioxide upto 800ºC. In Hydrogen Sulphide up to 550ºC.
SHIELDING GAS : Ar 99.99% , 16-21 l/min ; Ar +30% He, 20-25 l/min
PACKING PARAMETERS
Size (mm) | Weight / Spool (kg) |
0.8 | 15 |
1.2 | 15 |
1.6 | 15 |