IDENTIFICATION
GM ST-12, ER CCoCr-B
CLASSIFICATION
AWS/SFA 5.21: ER CCOCR-B
DESCRIPTION
GM ST12 content of complex carbides in an alloy matrix. They are resistant to wear & corrosion to retain these properties at high temperature. These wear resistance in mainly due to inherent characteristic of hard carbide phase.
CHEMICAL ANALYSIS (RANGE) %
C | Si | Cr | Ni | Mn | Mo | Fe | Co | W |
1.2 - 2.0 | 2.0 max | 25.0-32.0 | 3.0 max | 2.0 max | 1.0 max | 5.0 max | Bal. | 07-Oct |
TYPICAL APPLICATIONS
WELD METAL PROPERTIES
Hardness : 45 - 50 HRC
GENERAL CHARACTERISTICS
WELDING PARAMETERS
Diameter (mm) | Current intensity (A) | Voltage (V) | Stick-out (mm) | Gas flow | Weight / Spool (kg) |
(1/mm) | |||||
1.2 | 110 - 180 | 20 -31 | 20 max | Dec-15 | 12.5 / 15.0 |
1.6 | 150 - 250 | 20 - 31 | 20 max | Dec-15 | 12.5 / 15.0 |
2.40 / 2.50 | 300 - 400 | 24 - 31 | 20 max | 15 -20 | 12.5 / 15.0 |